Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.59 GPa @Strain 1.68 %, Temperature 0.000 °C |
811 ksi @Strain 1.68 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |