Mechanical Properties Metric English Comments
Secant Modulus 1.82 GPa

@Strain 3.50 %,
Temperature 100 °C
264 ksi

@Strain 3.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Secant Modulus 1.82 GPa

@Strain 0.900 %,
Temperature 100 °C
264 ksi

@Strain 0.900 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Secant Modulus 1.82 GPa

@Strain 2.40 %,
Temperature -20.0 °C
264 ksi

@Strain 2.40 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..