Polymer Property : Secant Modulus = 1.82 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 1.82 GPa

@Strain 0.950 %,
Temperature 0.000 °C
263 ksi

@Strain 0.950 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® BM6450XD BK560 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
Unreinforced Polybutylene Terephthalate Developed for Blow MoldingCrastin BM6450XD BK560 is an unreinforced supertough polybutylene terephthalate resin with very high viscosity for extrusion and blo..
Secant Modulus 1.82 GPa

@Strain 3.8646 %,
Temperature 0.000 °C
265 ksi

@Strain 3.8646 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F10 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin S600F10 NC010 is an unreinforced lubricated medium high viscosity polybutylene terephthal..
Secant Modulus 1.82 GPa

@Strain 3.50 %,
Temperature 100 °C
264 ksi

@Strain 3.50 %,
Temperature 212 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P..
Secant Modulus 1.82 GPa

@Strain 0.900 %,
Temperature 100 °C
264 ksi

@Strain 0.900 %,
Temperature 212 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66  (Unverified Data**)
40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Secant Modulus 1.82 GPa

@Strain 2.40 %,
Temperature -20.0 °C
264 ksi

@Strain 2.40 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..