Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.45 GPa @Strain 3.22 %, Temperature -40.0 °C |
356 ksi @Strain 3.22 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Secant Modulus | 2.45 GPa @Strain 3.22 %, Temperature -40.0 °C |
356 ksi @Strain 3.22 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT) Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided.. |
|||
Secant Modulus | 2.45 GPa @Strain 0.411103 %, Temperature 100 °C |
355 ksi @Strain 0.411103 %, Temperature 212 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |