Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.37 GPa @Strain 0.700 %, Temperature 23.0 °C |
344 ksi @Strain 0.700 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |
|||
Secant Modulus | 2.37 GPa @Strain 0.790 %, Temperature -40.0 °C |
344 ksi @Strain 0.790 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |