Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus = 2.25 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 2.25 GPa

@Strain 1.89 %,
Temperature 23.0 °C
326 ksi

@Strain 1.89 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l
Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi..
Secant Modulus 2.25 GPa

@Strain 1.89 %,
Temperature 23.0 °C
326 ksi

@Strain 1.89 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT)
Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided..
Secant Modulus 2.25 GPa

@Strain 2.40 %,
Temperature 0.000 °C
326 ksi

@Strain 2.40 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)  (Unverified Data**)
High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and ..
Secant Modulus 2.25 GPa

@Strain 1.09 %,
Temperature -40.0 °C
326 ksi

@Strain 1.09 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010
Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced..
Copyright © lookpolymers.com All Rights Reserved