Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 7.33 GPa @Strain 2.30 %, Temperature -20.0 °C |
1060 ksi @Strain 2.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS BK591 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for inject.. |
|||
Secant Modulus | 7.33 GPa @Strain 2.30 %, Temperature -20.0 °C |
1060 ksi @Strain 2.30 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HFS NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate with Improved Processing Crastin HR5330HFS is a 30% glass fiber reinforced moderately toughened hydrolysis resistant polybutylene terephthalate for in.. |
|||
Secant Modulus | 7.32 GPa @Strain 0.680 %, Temperature 23.0 °C |
1060 ksi @Strain 0.680 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70M30V0 NC010 Nylon 66
(Unverified Data**) 30% Mineral Reinforced Flame Retardant Polyamide 66 Zytel FR70M30V0 NC010 is a 30% mineral reinforced flame retardant polyamide 66 resin for injection molding.Information provided by DuPont Performa.. |
|||
Secant Modulus | 7.29 GPa @Strain 2.26 %, Temperature -20.0 °C |
1060 ksi @Strain 2.26 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |
|||
Secant Modulus | 7.29 GPa @Strain 3.13 %, Temperature -40.0 °C |
1060 ksi @Strain 3.13 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |
|||
Secant Modulus | 7.32 GPa @Strain 0.630 %, Temperature 23.0 °C |
1060 ksi @Strain 0.630 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |