Mechanical Properties Metric English Comments
Secant Modulus 10.3 GPa

@Strain 0.500 %,
Temperature 0.000 °C
1490 ksi

@Strain 0.500 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT)
30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol..
Secant Modulus 10.3 GPa

@Strain 1.30 %,
Temperature -40.0 °C
1490 ksi

@Strain 1.30 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66  (Unverified Data**)
43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information..
Secant Modulus 10.3 GPa

@Strain 0.500 %,
Temperature 0.000 °C
1490 ksi

@Strain 0.500 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)  (Unverified Data**)&
30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo..