Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.600 GPa | 87.0 ksi | ASTM D695 |
Quadrant EPP TIVAR® 88 ESD UHMW-PE, Premium Glass Filled, Crosslinked Electro Static Dissipative Lining Material (ASTM Product Data Sheet) |
|||
Compressive Modulus | 0.600 GPa | 87.0 ksi | ASTM D695 |
3M Dyneon™ CC191-HE PTFE, 25% Carbon/Graphite Filled
(discontinued **) Product Form: Black, non-pelletized powder. Applications include bearings, bushings.Data provided by Dyneon. |
|||
Compressive Modulus | 0.600 - 0.700 GPa @Strain 0.200 % |
87.0 - 102 ksi @Strain 0.200 % |
ASTM D621 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Compressive Modulus | 0.600 GPa | 87.0 ksi | Stabilized, typ |
Hexcel® HexWeb® HRH-327 - 3/16 - 6.0 Fiberglass Reinforced Polyimide Honeycomb Designation: Material-Cell Size (inches)-DensityHexWeb® HRH-327 is a glass-fabric, bias weave reinforced plastic honeycomb that incorporates a polyimide resin system for the node adhesive as well a.. |
|||
Compressive Modulus | 0.600 GPa | 87.0 ksi | Unloading, In the In Plane Direction |
Cymat A35620SC 020SS Stabilized Aluminum Foam Description: Cymat A35620SC 020SS stabilized aluminum foam (SAF) is a closed cell aluminum foam formed from A356 aluminum alloy with a density of 0.2 g/cm3. The mechanical properties of SAF make it .. |
|||
Compressive Modulus | 0.600 - 0.700 GPa @Strain 0.200 % |
87.0 - 102 ksi @Strain 0.200 % |
ASTM D621 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |