Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.138 - 4.14 GPa | 20.0 - 600 ksi | Average value: 2.97 GPa Grade Count:9 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Compressive Modulus | 2.41 - 4.14 GPa | 350 - 600 ksi | Average value: 2.86 GPa Grade Count:4 |
Overview of materials for Polyamide-Imide, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polyamide-Imide, Molded". Each property range of values reported is minimum and maximum values of approp.. |