Mechanical Properties Metric English Comments
Compressive Modulus 2.24 GPa
325 ksi
ASTM D695
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet)
Compressive Modulus 2.24 GPa
325 ksi
Inchem Phenoxy PKFE
Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation.
Compressive Modulus 2.24 GPa
325 ksi
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated
HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact..