Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 2.24 GPa | 325 ksi | ASTM D695 |
Quadrant EPP Nylatron® 4.6 (ASTM Product Data Sheet) |
|||
Compressive Modulus | 2.24 GPa | 325 ksi | |
Inchem Phenoxy PKFE Phenoxy PKFE - polyhydroxy ether of Bisphenol A. Originally developed by Union Carbide. Produced by InChem Corporation. |
|||
Compressive Modulus | 2.24 GPa | 325 ksi | |
CMT Materials HYTAC® WFT High Temperature, Ultra-Smooth PTFE Impregnated HYTAC-WFT combines the higher temperature, smooth surface properties of HYTAC-WF with PTFE impregnation for low stick surface capability and excellent material distribution. The result is a syntact.. |