Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.65 GPa | 240 ksi | |
Engineered Syntactic Systems BZ-30 Deep Water Syntactic Foam Syntactic foams are a unique combination of hollow spheres, a resin matrix, and other additives. When combined and processed properly, the constituents form a lightweight homogeneous material having.. |
|||
Compressive Modulus | 1.65 GPa | 240 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 1/8-5052-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 1.65 GPa | 240 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 1/8-5052-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 1.65 GPa | 240 ksi | Stabilized, typ |
Hexcel® HexWeb® CR III 5/32-5056-.0015 Corrosion Resistant Specification Grade Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge."5052 and 5056 expanded aerospace grade aluminum honeycomb materials are available in a wide selection of cell sizes and foil gauges. The HexWeb CR.. |
|||
Compressive Modulus | 1.65 GPa | 240 ksi | Stabilized, typ |
Hexcel® HexWeb® CR-PAA™ 5/32-5056-0.0015 Phosphoric Acid Anodized Aluminum Honeycomb Grade is designated as "Cell Size-Alloy-Foil Gauge." The life cycle of aluminum honeycomb sandwich structures in a given application can be directly related to the quality of the bond between the fa.. |
|||
Compressive Modulus | 1.65 GPa | 239 ksi | |
Abatron AboCast 50-11/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 240 min. at 25°C(77°F). Exothermic Peak 190°C (375°F). Hardens in 2-24 hours.. |
|||
Compressive Modulus | 1.65 GPa | 239 ksi | |
Abatron AboCast 50-16/AboCure 50-1 Epoxy Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 380 min. at 25°C (77°F). Exothermic Peak 154°C (310°F). Hardens in 2-24 hour.. |
|||
Compressive Modulus | 1.65 GPa | 239 ksi | |
Abatron AboCast 50-6/AboCure 50-1 Epoxy Data provided by the manufacturer, Abatron, Inc. Motor oil viscosity, light amber color. Peak exothermic temperature is 160°C (320°F). Shelf life is 12+ months. |