Abatron AboCast 50-16/AboCure 50-1 Epoxy

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Abatron
Trade Name AboCast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboCast 50-16/AboCure 50-1 Epoxy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Abatron, Inc.Processing: Shelf life: 12+ months (unmixed). 100/35 ratio. Pot life: 500 g, 380 min. at 25°C (77°F). Exothermic Peak 154°C (310°F). Hardens in 2-24 hours at RT (faster with heat). Full cure in 1-5 weeks at RT or 1-4 hrs at 80-120°C (175-250°F).
Physical Properties Metric English Comments
Viscosity Measurement 700
700
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
Tensile Strength, Ultimate 47.09 MPa
6830 psi
Elongation at Break 9.1 %
9.1 %
Flexural Yield Strength 64.8 MPa
9400 psi
Flexural Modulus 1.96 GPa
284 ksi
Compressive Yield Strength 63.36 MPa
9190 psi
Compressive Modulus 1.65 GPa
239 ksi
Izod Impact, Notched 0.342 J/cm
0.641 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 58.0 °C
136 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 3.43e+15 ohm-cm
3.43e+15 ohm-cm
Surface Resistance 4.71e+15 ohm
4.71e+15 ohm
Dielectric Constant 2.92

@Frequency 1e+6 Hz
2.92

@Frequency 1e+6 Hz
3.12

@Frequency 1000 Hz
3.12

@Frequency 1000 Hz
3.17

@Frequency 60 Hz
3.17

@Frequency 60 Hz
Dissipation Factor 0.0089

@Frequency 1000 Hz
0.0089

@Frequency 1000 Hz
0.010

@Frequency 60 Hz
0.010

@Frequency 60 Hz
0.018

@Frequency 1e+6 Hz
0.018

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Pot Life 380 min
380 min
500 g
Descriptive Properties Value Comments
Exotherm 154°C
Peak