Polymer Property : Compressive Modulus = 1.39 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 0.00960 GPa
1.39 ksi
0.1; ASTM D695
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability
Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo.