Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 0.00960 GPa | 1.39 ksi | 0.1; ASTM D695 |
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |