Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 6.89 MPa @Strain 1.00 % |
999 psi @Strain 1.00 % |
ASTM D695 |
Saint-Gobain Fluoroloy® A12 High Performance Seal Material Excellent wear and heat resistance; Non-abrasive; Recommended for moderate to high speed service running against soft or hard metals; Performs well against lubricated and non-lubricated surfacesInfo.. |
|||
Compressive Yield Strength | 6.89 MPa @Strain 1.00 % |
999 psi @Strain 1.00 % |
ASTM D695 |
Saint-Gobain Fluoroloy® A08 High Performance Seal Material Superior heat and wear resistance; Recommended for moderate to high speed dynamic service running against soft metals; Non-abrasive
Information provided by Saint-Gobain Performance Plastics. |