Material Notes:
Superior heat and wear resistance; Recommended for moderate to high speed dynamic service running against soft metals; Non-abrasive Information provided by Saint-Gobain Performance Plastics.
Physical Properties Metric English Comments
Density 2.03 g/cc
0.0733 lb/in³
ASTM D792
Deformation 8.3 %

@Time 86400 sec
8.3 %

@Time 24.0 hour
13.8 MPa (2000 psi) load; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength 20.7 MPa
3000 psi
ASTM D4894
Elongation at Break 230 %
230 %
ASTM D4894
Tensile Modulus 0.379 GPa
55.0 ksi
ASTM D4894
Compressive Yield Strength 6.89 MPa

@Strain 1.00 %
999 psi

@Strain 1.00 %
ASTM D695
Compressive Modulus 0.655 GPa
95.0 ksi
ASTM D695
Coefficient of Friction 0.20
0.20
ASTM D3702
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 127 µm/m-°C

@Temperature 26.0 - 200 °C
70.6 µin/in-°F

@Temperature 78.8 - 392 °F
Mold Direction; ASTM D696
CTE, linear, Transverse to Flow 132 µm/m-°C

@Temperature 26.0 - 200 °C
73.3 µin/in-°F

@Temperature 78.8 - 392 °F
ASTM D696
Maximum Service Temperature, Air 288 °C
550 °F
Minimum Service Temperature, Air -268 °C
-450 °F
Descriptive Properties Value Comments
Color Tan