Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 48.3 MPa | 7000 psi | Mixed 1:1; TM R050-38 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Compressive Yield Strength | 48.3 - 58.6 MPa | 7000 - 8500 psi | Average value: 53.4 MPa Grade Count:4 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini.. |
|||
Compressive Yield Strength | 48.3 MPa | 7000 psi | TM R050-38 |
Resinlab® EP1046FG Black Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Black is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Yield Strength | 48.3 MPa | 7000 psi | TM R050-38 |
Resinlab® EP1046FG Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP1046FG Clear is a two part unfilled very fast curing electronic grade epoxy encapsulant designed for small castings (less than 25 grams). It cures very quickly with low exotherm to a to.. |
|||
Compressive Yield Strength | 48.3 - 170 MPa | 7000 - 24700 psi | Average value: 71.2 MPa Grade Count:7 |
Overview of materials for Polypropylene with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i.. |