Mechanical Properties Metric English Comments
Compressive Yield Strength 48.3 - 58.6 MPa
7000 - 8500 psi
Average value: 53.4 MPa Grade Count:4
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), NCG Fiber Filled". Each property range of values reported is mini..