Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 270 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 270 MPa
39200 psi
Compression strength after impact, 20J
Hexcel® HexPly® M36/NC2 180°C (350°F) Curing Epoxy Matrix, Multiaxial Fabric Laminate (NC2)
Uses Hexcel NC2 non-crimp fabric based on Tenax HTS fiber; Quasi-isotropic lay-up based on 1072 gsm quadaxial NC2 fabric (267 gsm/ply); Laminates manufactured via resin film infusionInformation prov..
Compressive Yield Strength 270 MPa
39200 psi
Cytec Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco ..
Copyright © lookpolymers.com All Rights Reserved