Cytec Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite , Filled/Reinforced Thermoset
Manufacturer Cytec
Trade Name Thornel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Cytec Thornel® P-120 Carbon Fiber/Epoxy Advanced Composite System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Amoco Performance Products, Inc. Measured in proprietary aerospace grade epoxy formulations at 0.62 fiber content by volume.Thornel® products were sold by Amoco and are now owned by Cytec.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1210 MPa
175000 psi
Tensile Modulus 520 GPa
75400 ksi
Compressive Yield Strength 270 MPa
39200 psi
Shear Strength 30.0 MPa
4350 psi
Thermal Properties Metric English Comments
Thermal Conductivity 400 W/m-K
2780 BTU-in/hr-ft²-°F