Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.00200 - 0.00462 MPa @Strain 25.0 % |
0.290 - 0.670 psi @Strain 25.0 % |
0.2"/min. strain rate, varies with thickness |
Rogers Corporation Poron® 4701-15 Urethane Foam, Soft Seal PORON® 4701-15 Improved Soft Seal SeriesEnhanced Surface Toughness, Reliable Materials for Thinner DesignsIncreased Surface Toughness, Improved YieldsExcellent Compressibility and ConformabilityLon.. |