Mechanical Properties Metric English Comments
Compressive Yield Strength 0.00200 - 0.00462 MPa

@Strain 25.0 %
0.290 - 0.670 psi

@Strain 25.0 %
0.2"/min. strain rate, varies with thickness
Rogers Corporation Poron® 4701-15 Urethane Foam, Soft Seal
PORON® 4701-15 Improved Soft Seal SeriesEnhanced Surface Toughness, Reliable Materials for Thinner DesignsIncreased Surface Toughness, Improved YieldsExcellent Compressibility and ConformabilityLon..
Compressive Yield Strength 0.00200 MPa

@Strain 25.0 %
0.290 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Porocell POR 304 CM-OPC EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.