Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 59.6 kN/m | 340 pli | Die C; ASTM D624 |
Lubrizol Estane® ZHF 95AT3 Thermoplastic Polyurethane, Flame Retardant Type: Estane® ZHF 95AT3 TPU is a zero halogen flame retardant polyether based thermoplastic polyurethane compound.Features: Outstanding flame retardant properties, especially suited for tray cables.. |
|||
Graves Tear Strength | 59.6 kN/m | 340 pli | Die C; ASTM D624 |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,.. |
|||
Graves Tear Strength | 59.6 kN/m | 340 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58810 Ether Based Thermoplastic Polyurethane Features: High melt flow and improved temperature resistanceUses: Extrusion – Wire and cable, Hose and tubeAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by .. |
|||
Graves Tear Strength | 59.6 kN/m | 340 pli | Die C, perpendicular flow; ASTM D624 |
Advanced Polymer Alloys DuraGrip™ 6165 TR Thermoplastic Elastomer DuraGrip® DGR6165TR is a translucent thermoplastic elastomer (TPE) formulated for excellent elastic properties and enhanced adhesion to engineered thermoplastics using insert molding, co-injection .. |