Polymer Property : Graves Tear Strength = 170 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 29.8 kN/m
170 pli
PVC (80)/CP80AS2(20)
Lubrizol Estane® CP80AS2 Thermoplastic Polyurethane
Type: Estane® CP80AS2 is a soft, polyester based thermoplastic polyurethane resin.Features: Outstanding compatibility with flexible PVC allowing easy dispersion without pre-compounding.Uses: Tube/H..
Graves Tear Strength 29.8 kN/m

@Temperature 23.9 °C
170 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 2070 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 29.8 kN/m

@Temperature 24.0 °C
170 pli

@Temperature 75.2 °F
Die C; ASTM D624
Advanced Polymer Alloys DuraGrip™ DGR 6150 NC Thermoplastic Elastomer (TPE)
DuraGrip® DGR 6150 is offered in an NC (colorable) version, and is designed to chemically bond to a wide variety of thermoplastic substrates including ABS, PC, Nylon 6, Nylon 6/6, glass filled Nylo..
Graves Tear Strength 29.8 kN/m

@Temperature 23.9 °C
170 pli

@Temperature 75.0 °F
Die C; ASTM D624
Advanced Polymer Alloys Alcryn® 4660 NC Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..
Graves Tear Strength 29.8 - 154 kN/m
170 - 880 pli
Average value: 78.2 kN/m Grade Count:5
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyester Grade
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyester Grade". Each property range of values reported is minimum a..