Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 9250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 63.8 MPa
9250 psi
ASTM D790-95
Multibase Multi-ABS 3832 Natural
Multi-ABS 3832 is specially formulated for ease of processability, controllability, and thin-walled parts where higher than normal temperatures are being used. This product also shows higher than n..
Flexural Strength 63.8 MPa
9250 psi
ASTM D790-95
Multibase Multi-ABS 801 Natural Extrusion Grade
Data provided by Multibase.
Flexural Strength 63.8 MPa
9250 psi
ASTM D790
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound
Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It ..