Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-ABS 3832 Natural

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Multibase
Trade Name Multi-ABS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-ABS 3832 Natural.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Multi-ABS 3832 is specially formulated for ease of processability, controllability, and thin-walled parts where higher than normal temperatures are being used. This product also shows higher than normal impacts, both notched izod and gardner, than typical High Heat ABS.Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.05 g/cc
0.0379 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.0080 cm/cm
0.0080 in/in
ASTM D955-89
Melt Flow 2.0 g/10 min
2.0 g/10 min
(Condition I) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 41.4 MPa
6000 psi
ASTM D638-95
Elongation at Break 50 %
50 %
ASTM D638-95
Flexural Strength 63.8 MPa
9250 psi
ASTM D790-95
Flexural Modulus 2.379 GPa
345.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 1.87 J/cm
3.50 ft-lb/in
ASTM D256-93a
Gardner Impact 19.8 J
14.6 ft-lb
ASTM D5420-93
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648-95
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648-95