Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 63.8 MPa | 9250 psi | ASTM D790-95 |
Multibase Multi-ABS 3832 Natural Multi-ABS 3832 is specially formulated for ease of processability, controllability, and thin-walled parts where higher than normal temperatures are being used. This product also shows higher than n.. |
|||
Flexural Strength | 63.8 MPa | 9250 psi | ASTM D790-95 |
Multibase Multi-ABS 801 Natural Extrusion Grade Data provided by Multibase. |
|||
Flexural Strength | 63.8 MPa | 9250 psi | ASTM D790 |
Chesterton ARC BX2 Contractor Grade Fine Sliding Wear Compound Description: ARC BX2 is an advanced contractor grade ceramic reinforced composite for the repair and protection of all metal surfaces subjected to severe erosion, corrosion, and chemical attack. It .. |