Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 5900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 40.7 MPa
5900 psi
Conditioned; ASTM D790
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6
Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi..
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000EL Nylon 6/6 (Cond)  (discontinued **)
Information provided by Ravago.
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Fibre Glast 1099 Room Temperature Epoxy Surface Coat
Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that c..
Flexural Strength 40.7 MPa

@Temperature 1500 °C
5900 psi

@Temperature 2730 °F
Perpendicular
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite
Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu..
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate
Information provided by FIBERFIL Engineered Plastics
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Techmer ES HiFill® ASA 778 UV WT168
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc.
Flexural Strength 40.7 MPa
5900 psi
Injection Molded; ASTM D790
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin
Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati..
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Chase Plastics CP Pryme® N100MD2 (COND, 50% RH) Nylon 6 with 2% MoS2 Lubricated
Information provided by Chase Plastics.
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Chesterton ARC MXC Castable Extreme Wear Compound
Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro..
Flexural Strength 40.7 MPa
5900 psi
ASTM D790
Chase Plastics CP Pryme® PE200-HD20M General Purpose High Density Polyethylene
Information provided by Chase Plastics.