Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 40.7 MPa | 5900 psi | Conditioned; ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000HL Nylon 6/6 Available in North America Additive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and Lubricated RoHS Compliant Auto Specifications: FORD WSK-M4D648-A Color: Black Form: Pellets Processi.. |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000 Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EHL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1000EL Nylon 6/6 (Cond)
(discontinued **) Information provided by Ravago. |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Fibre Glast 1099 Room Temperature Epoxy Surface Coat Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours. #1099 is a white, medium viscosity epoxy surface coat that c.. |
|||
Flexural Strength | 40.7 MPa @Temperature 1500 °C |
5900 psi @Temperature 2730 °F |
Perpendicular |
Momentive Performance Materials BNC1 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Fiberfil® PP-60/CC/20 Polypropylene Homopolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Techmer ES HiFill® ASA 778 UV WT168 Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Good UV ResistanceAppearance: WhiteInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 40.7 MPa | 5900 psi | Injection Molded; ASTM D790 |
Styron STYRONâ„¢ 6500 Ignition Resistant Polystyrene Resin Overview: STYRONâ„¢ 6500 is an ignition-resistant polystyrene resin with excellent balance of strength, heat resistance and flow properties that are tailor-made for consumer electronics applicati.. |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Chase Plastics CP Pryme® N100MD2 (COND, 50% RH) Nylon 6 with 2% MoS2 Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Chesterton ARC MXC Castable Extreme Wear Compound Description: An advanced ceramic composite, with flowable viscosity, for the repair and protection of all metal surfaces subjected to severe erosion, abrasion and chemical attack. It can be hand tro.. |
|||
Flexural Strength | 40.7 MPa | 5900 psi | ASTM D790 |
Chase Plastics CP Pryme® PE200-HD20M General Purpose High Density Polyethylene Information provided by Chase Plastics. |