Flexural Strength | 354 MPa | 51300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant. |
|||
Flexural Strength | 354 MPa | 51300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 354 MPa | 51300 psi | ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East) LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 354 MPa | 51300 psi | ASTM D790 |
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |