Mechanical Properties Metric English Comments
Flexural Strength 354 MPa
51300 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Flexural Strength 354 MPa
51300 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 354 MPa
51300 psi
ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
Flexural Strength 354 MPa
51300 psi
ASTM D790
Saint-Gobain Meldin® 5330 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..