Polymer Property : Flexural Strength = 49.05 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 49.05 MPa
7114 psi
Shinil Chemical SHINSTAT PCTG Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Flexural Strength 49.05 MPa
7114 psi
Shinil Chemical SHINSTAT PE Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Flexural Strength 49.05 MPa
7114 psi
ASTM D790
E-Polymers TEKAFIN® PH40FR2 Flame Retardant Heat Resistance Compounded-PP
Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.I..