Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

E-Polymers TEKAFIN® PH40FR2 Flame Retardant Heat Resistance Compounded-PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Flame Retardant
Manufacturer E-Polymers Co. Ltd.
Trade Name TEKAFIN®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF E-Polymers TEKAFIN® PH40FR2 Flame Retardant Heat Resistance Compounded-PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Modified PP: TEKAFIN is modified PP resins formulated with various fillers and modifiers. It has product lines for impact modified, glass fiber reinforced, inorganic filler reinforced and hybrids.Information Provided by E-Polymers Co., Ltd.
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Linear Mold Shrinkage 0.016 cm/cm
0.016 in/in
Mechanical Properties Metric English Comments
Tensile Strength 34.335 MPa
4979.9 psi
ASTM D638
Elongation at Break 40 %
40 %
ASTM D638
Flexural Strength 49.05 MPa
7114 psi
ASTM D790
Flexural Modulus 1.6677 GPa
241.88 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 120 °C
248 °F
ASTM D648
Flammability, UL94 V-2
V-2
Processing Properties Metric English Comments
Melt Temperature 170 - 200 °C
338 - 392 °F
Mold Temperature 40.0 - 60.0 °C
104 - 140 °F
Copyright © lookpolymers.com All Rights Reserved