Shinil Chemical SHINSTAT PCTG Electrostatic Control Polymer Sheet Grade

Category Polymer , Thermoplastic , Polyester, TP , Polycyclohexylenedimethylene Terephthalate (PCT) , Glycol-Modified PCT (PCTG) Copolyester
Manufacturer Shinil Chemical
Trade Name SHINSTAT
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shinil Chemical SHINSTAT PCTG Electrostatic Control Polymer Sheet Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for special polymers (PC, PETG, PCTG, PS, ABS, PC/ABS, PMMA etc) to impart permanent static dissipative property. SHINSTAT is directly molded or extruded (film) to achieve the desired level of antistatic property. The level of surface resistivity by SHINSTAT can be varied in the final products depending upon customer needs.Feature and BenefitsPermanent electrostatic controllabilityTransparent and colorableLess humidity dependentNo particulatesLow ionics, out gassing or bloomingRecyclabilityUsed for injection molding, film or sheet extrusionCost effectiveInformation Provided by Shinil Chemical Industry Co., Ltd.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 39.2 MPa
5690 psi
Flexural Strength 49.05 MPa
7114 psi
Flexural Modulus 1.67 GPa
242 ksi
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
Optical Properties Metric English Comments
Transmission, Visible 82 %
82 %
Electrical Properties Metric English Comments
Volume Resistivity 6.00e+9 ohm-cm
6.00e+9 ohm-cm
Processing Properties Metric English Comments
Processing Temperature 210 °C
410 °F