Mechanical Properties Metric English Comments
Flexural Strength 333 MPa
48300 psi
ASTM D790
Kolon KOPA® KN333G45 G/F Reinforced Nylon 66
G/F 45% reinforcedApplications Internal gearsInformation provided by API-Kolon.
Flexural Strength 333 MPa
48300 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this material include: Electrically Conductive, Wear Resistant.
Flexural Strength 333 MPa
48300 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Asia Pacific)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Silicone, PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.
Flexural Strength 333 MPa
48300 psi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP RCP36 PA 66 (Europe-Africa-Middle East)
LNP LUBRICOMP* RCP36 is a compound based on Nylon 66 resin containing Carbon Fiber, Silicone, PTFE. Added features of this material include: Electrically Conductive.
Flexural Strength 333 MPa
48300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Strength 333 MPa
48300 psi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® MKD-1016 PA, 55% Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Strength 333 MPa
48300 psi
ISO 178
Vyncolit Vyntec® CF8050 Carbon Fiber Reinforced Phenolic
VYNTEC CF8030 is a carbon fiber reinforced phenolic moldable composite with excellent tribological properties. It has high mechanical strength combined with low density.Information provided by Sumit..