Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Strength = 48000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 331 MPa
48000 psi
ASTM D790
PolyOne Stat-Tech™ NN-30CF/000 Black Polyamide 66 (Nylon 66)
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound..
Flexural Strength 331 MPa
48000 psi
1.3 mm/min; ASTM D790
PolyOne Stat-Tech™ NN-40CF/000 FRV0 Natural Polyamide 66 (Nylon 66)
Information provided by PolyOne
Flexural Strength 331 MPa
48000 psi
ASTM D-790
PlastiComp Complet® LGF40-PPA Polyphthalamide, 40% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 40% long glass fiber reinforcementInformation provided by PlastiC..
Flexural Strength 331 MPa
48000 psi
1.3 mm/min; ASTM D790
PolyOne Edgetek® NN-40CF/000 FRV0 NATURAL Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Flexural Strength 331 MPa
48000 psi
ASTM D790
PolyOne Nymax™ GF 1200 60 HS Black 22 Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Flexural Strength 331 MPa
48000 psi
ASTM D-790
PlastiComp Complet® LCF40-PEI Polyetherimide, 40% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyetherimide with 40% long carbon fiber reinforcementInformation provided by PlastiC..
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 4085 A TFE 15 (Hot Water Moldable) Polyphthalamide (PPA), Carbon Fiber - PTFE Lubricated
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 2285 LF Z Polyetheretherketone (PEEK), Low Flow - Carbon Fiber - FDA Compliant Ingredients  (d
Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company VLF 80209 A Nylon 6 (PA), Long Glass Fiber
Flexural Strength 331 MPa
48000 psi
MTI ThermoStran® PA66-40G Long Glass Fiber Compound
ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t..
Flexural Strength 331 MPa
48000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF50 HS L BK 50% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
Flexural Strength 331 MPa
48000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF50 L UV 50% Glass Filled (Dry)
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformat..
Flexural Strength 331 - 345 MPa
48000 - 50000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF50 X 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeighTPCI# 10065101Information provided by TP Composites, Inc.
Flexural Strength 331 MPa
48000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF50 X BK 50% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightAppearance: BlackTPCI# 6560101Information provided by TP Composites, Inc.
Flexural Strength 331 MPa
48000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF60 HS L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N..
Flexural Strength 331 MPa
48000 psi
ASTM D790
Techmer ES HiFill® PA6/6 GF60 X 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedUL File N..
Flexural Strength 331 MPa
48000 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RC004SXS PA 66
LNP* THERMOCOMP* RC004SXS is a compound based on Nylon 66 containing 20% Carbon Fiber. Added feature of this grade includes: Heat Stabilized, Electrically Conductive.
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company ESD 4080 Polyphthalamide (PPA), Carbon Fiber - Electrically Conductive - ESD Protection
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 2283 HF Polyetheretherketone (PEEK), Carbon Fiber - High Flow
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 2283 LF Polyetheretherketone (PEEK), Carbon Fiber - Low Flow
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 285 FR Nylon 6/6 (PA), Carbon Fiber - Flame Retardant
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 285 TFE 5 Nylon 6/6 (PA), Carbon Fiber - PTFE Lubricated
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 287 A Nylon 6 (PA); Carbon Fiber
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 211 Nylon 6/6 (PA), Glass Fiber
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 285 A Nylon 6 (PA); Carbon Fiber
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 289 TFE 10 Nylon 6/6 (PA), Carbon Fiber - PTFE Lubricated
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 2387 A Rigid Thermoplastic Polyurethane (RTPU), Carbon Fiber
Flexural Strength 331 MPa
48000 psi
ASTM D 790
RTP Company RTP 4285 Thermoplastic Polyimide (TPI) Carbon Fiber
Flexural Strength 331 MPa
48000 psi
ASTM D790
PolyOne Edgetek® PI-40CF/000 Polyetherimide (PEI), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Flexural Strength 331 MPa
48000 psi
ASTM D790
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced  (discontinued **)
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved