PlastiComp Complet® LGF40-PPA Polyphthalamide, 40% Long Glass Fiber Reinforced

Category Polymer , Thermoplastic , Polyphthalamide (PPA) , Polyphthalamide (PPA), 40% Glass Fiber Reinforced
Manufacturer PlastiComp
Trade Name Complēt®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PlastiComp Complet® LGF40-PPA Polyphthalamide, 40% Long Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyphthalamide with 40% long glass fiber reinforcementInformation provided by PlastiComp, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.57 g/cc
1.57 g/cc
ASTM D-792
Filler Content 40 %
40 %
Long Glass Fiber
Mechanical Properties Metric English Comments
Tensile Strength 224 MPa
32500 psi
ASTM D-638
Elongation at Break 1.0 - 2.0 %
1.0 - 2.0 %
ASTM D-638
Tensile Modulus 14.828 GPa
2150.6 ksi
ASTM D-638
Flexural Strength 331 MPa
48000 psi
ASTM D-790
Flexural Modulus 13.793 GPa
2000.5 ksi
ASTM D-790
Izod Impact, Notched 2.67 J/cm
5.00 ft-lb/in
ASTM D-256
Izod Impact, Unnotched 11.21 J/cm
21.00 ft-lb/in
ASTM D-4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 277 °C
531 °F
ASTM D-648