Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 207 - 241 MPa | 30000 - 35000 psi | |
Bulk Molding Compounds BMC 680 Mineral Filled, Glass Fiber Reinforced Polyester Compound BMC 680 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression and stuffer injection molding It is characterized by good moldability, very high impa.. |