Mechanical Properties Metric English Comments
Flexural Strength 2220 MPa
322000 psi
China Tungsten ZP35 Tungsten Carbide
A versatile grade High in red hardness, strength in use and resistance to impact and thermal shocking. Roughing and strength cutting of steel and cast steel.Information provided by China Tungsten