Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 2220 MPa | 322000 psi | |
China Tungsten ZP35 Tungsten Carbide A versatile grade High in red hardness, strength in use and resistance to impact and thermal shocking. Roughing and strength cutting of steel and cast steel.Information provided by China Tungsten |