China Tungsten ZP35 Tungsten Carbide

Category Ceramic , Carbide
Manufacturer China Tungsten
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF China Tungsten ZP35 Tungsten Carbide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A versatile grade High in red hardness, strength in use and resistance to impact and thermal shocking. Roughing and strength cutting of steel and cast steel.Information provided by China Tungsten
Physical Properties Metric English Comments
Density 12.7 g/cc
0.459 lb/in³
Mechanical Properties Metric English Comments
Hardness, Rockwell A 91
91
Flexural Strength 2220 MPa
322000 psi