Polymer Property : Flexural Strength = 26.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength <= 26.0 MPa
<= 3770 psi
ISO 178
Polykemi AB POLYelast TPE ZC100 D40 Thermoplastic Elastomer
Information provided by Polykemi AB
Flexural Strength 26.0 MPa
3770 psi
across grain
Pyrotek PT-10 Graphite
PT-10 Graphite offers the highest resistance to oxidation available. Its unique composition gives it the most durable, long lasting, oxidation resistant properties available from treated graphite.A..
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
SABIC BM1052 High Density Polyethylene for Blow Molding
Product Description: BM1052 grade is a high molecular weight High Density Polyethylene copolymer with broad molecular weight distribution. It has excellent processability and exhibits very high im..
Flexural Strength 26.0 MPa
3770 psi
ASTM D790M
DSM Somos® 8120 Epoxy Photopolymer  (discontinued **)
DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and ..
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
LG Chemical LUPOL TE-5108 Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Flow
LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem
Flexural Strength 26.0 MPa
3770 psi
Kuraray HYBRAR® PP2 Thermoplastic Rubber-Polypropylene Blend
Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb..
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON FX98500 PE
LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific)
LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Flexural Strength 26.0 MPa
3770 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Strength 26.0 MPa
3770 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TH0750A PUR (Asia Pacific)
LNP THERMOCOMP* TH0750A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity.
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific)
LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive.
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON FX98500C PE
LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive.
Flexural Strength 26.0 MPa
3770 psi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU
LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber.
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
UBE 7128B Nylon 6/12 Copolymer
Description: UBESTA Nylon 12 CopolymerInformation provided by UBE.
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
UBE UBESTA® 3030JI9L Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: meet DIN73378 PHLYInformation provided by UBE.
Flexural Strength 26.0 MPa
3770 psi
ISO 178
Polyplastics Duracon® TD-35 Acetal Co-polymer (POM), High impact, Flexible
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
UBE UBESTA® 3030JLX2 Plasticized Automotive Grade Nylon 12
Description: UBE UBESTA® Automotive grade Nylon 12Comments: semi-plasticized, UV resistance, heat resistanceInformation provided by UBE.
Flexural Strength 26.0 MPa
3770 psi
cond; ISO 178
DSM Novamid® ST220 NAT PA6-I
Impact Modified, Injection Molding, Medium Viscosity
Flexural Strength 26.0 MPa
3770 psi
high temp bending
China-Yixing Longly Refractories Push Slab Semi-Corundum-Mullite
Our company's production of a variety of corundum mullite push slab (moved plate), corundum-mullite seggar, corundum mullite corrugated board and other kinds of the kiln furniture, high refractorine..
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436C40L Calcium Reinforced
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436W30L Wollastonite Reinforced
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436W30L1 Wollastonite Reinforced
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0436W40L Wollastonite Reinforced
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0437M40CL Mica Reinforced Coupled
Flexural Strength 26.0 MPa
3770 psi
ASTM D790
A. Schulman ComAlloy Comtuf® 109 Polypropylene, Mineral Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i..
Flexural Strength 26.0 MPa
3770 psi
ISO 178
Unitika EX-1222 PA6, Conditioned
High-impact nylonInformation provided by Unitika Ltd.
Flexural Strength 26.0 MPa
3770 psi
0.1 in/min; ASTM D790
Ineos Nova Zyntar® 779 High Performance Flame Retardant Polystyrene  (discontinued **)
Non-Decabromodiphenyl Oxide, Color stable, Custom colorsApplications: Injection molding, Alternative to flame retardant ABS, Copiers, Computer monitors, Office equipmentThis is an impact grade of po..