Mechanical Properties Metric English Comments
Flexural Strength 117 - 131 MPa
17000 - 19000 psi
ASTM D790
Mar-Bal MB5500 Thermoset Polyester Composite Molding Compound
A superior heat resistant material. U.L. RTI rating of 160°C-170°C.Mar-Bal standard grades can be injection, compression and transfer molded.Information provided by Mar-Bal, Inc.
Flexural Strength 103 - 131 MPa
15000 - 19000 psi
Bulk Molding Compounds BMC G10(12) Mineral Filled, Glass Fiber Reinforced Polyester
BMC G10 is a general purpose, mineral filled, glass fiber-reinforced polyester that is suitable for compression, transfer and stuffer injection molding. G10 is well suited to applications where hig..
Flexural Strength 103 - 131 MPa
15000 - 19000 psi
Bulk Molding Compounds BMC T15(F) High Strength Grade Molding Compound
BMC T15F is a high strength, low shrink general purpose molding compound. Due to the excellent flow and controlled reactivity, BMC T15F is well suited for injection, transfer or compression molding..