Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 10.3 - 17.2 MPa | 1500 - 2500 psi | @ 5% strain; ASTM D790 |
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |