Flexural Strength 10.3 MPa
1500 psi
Cotronics Resbond™ 906 High Temperature Ceramic Adhesive, High Expansion
Flexural Strength 10.3 MPa
1500 psi
Cotronics Resbond™ 931 High Temperature Graphite Adhesive
Flexural Strength 10.3 - 17.2 MPa
1500 - 2500 psi
@ 5% strain; ASTM D790
Arkema Group Kynar Super Flex® 2500 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..