Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 0.370 MPa | 53.7 psi | 32 hour silo aging time, 20 kg/m^3 |
Jackon JACKOCELL® R411 Expanded Polystyrene Packaging and Shape Molding 100% Polystyrene.Pre-expansionThe unique design of polystyrene chains and additive chemistry in the Jackocell® R411 gives pre-expanded beads of high dimensional stability. The R411 represents the.. |
|||
Flexural Strength | 0.370 MPa | 53.7 psi | after 24 hrs at 1200°C, as Received, Parallel to Thickness |
Zircar Ceramics ASQ Castertip 14 pcf density refractory ceramic fiber "soft tip". Alumina bonding of shot free fiber results in extreme performance in manufacture of the finest grades of medical, food and packaging foils. Inform.. |