Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.74 MPa @Strain 15.77 %, Temperature 60.0 °C |
833 psi @Strain 15.77 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.74 MPa @Strain 0.230 %, Temperature -20.0 °C |
833 psi @Strain 0.230 %, Temperature -4.00 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |