Polymer Property : Tensile Stress = 8050 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 55.5 MPa

@Strain 4.62 %,
Temperature -20.0 °C
8050 psi

@Strain 4.62 %,
Temperature -4.00 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 55.50 MPa

@Strain 0.700 %,
Temperature -40.0 °C
8050 psi

@Strain 0.700 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..